We tested our walls with the demolition ball. Some groups walls started
to break apart after 2 to 3 hits. A couple of groups made it to the
level 4 with 2 hits at that level. We then analyzed all the walls and
talked about what made those successful. Both of the groups that made it
to the level 4 had a mortar mixture that was 2 clay and one sand. One
group used 4 Tablespoons water and the other group used 5
Tablespoons. Both groups used a large rock on the bottom design. We then took the
information from our observations and created our redesign for our
mortar and wall plan for tomorrow.